Bonding neat hydrophobic-rich resins to etched dentin: A proof of concept

Stape; Thiago Henrique Scarabello; Ismail, Omar Abdelaziz; Capitanio, Marcelo; Tezvergil-Mutluay, Arzu

Bonding neat hydrophobic-rich resins to etched dentin: A proof of concept

Stape
Thiago Henrique Scarabello
Ismail, Omar Abdelaziz
Capitanio, Marcelo
Tezvergil-Mutluay, Arzu
Katso/Avaa
1-s2.0-S0109564124003087-main.pdf (4.257Mb)
Lataukset: 

Elsevier Inc.
doi:10.1016/j.dental.2024.10.018
URI
https://doi.org/10.1016/j.dental.2024.10.018
Näytä kaikki kuvailutiedot
Julkaisun pysyvä osoite on:
https://urn.fi/URN:NBN:fi-fe2025082787581
Tiivistelmä

Objectives: To examine whether the effectiveness of current dentin-priming approaches requiring solvated hydrophilic resins may be replicated by modifying the infiltration dynamics of neat methacrylate-based monomers into dry-etched dentin using dimethyl sulfoxide (DMSO) pretreatments.

Methods: H3PO4-etched mid-coronal dentin surfaces from human molars were air-dried for 30 s and randomly pretreated with 50 %(v/v) ethanolic DMSO for 20 or 60 s. Untreated samples and an isolated wet-bonding group served as controls. Samples were bonded with a three-step etch-and-rinse adhesive or simply with the solvent-free hydrophobic-rich resin. Restored crown segments (n = 7/group) were stored in distilled water for 24 h and sectioned for microtensile bond strength testing. Resin-dentin beams (0.8 mm2) were tested under tension until failure (0.5 mm/min) after 24 h or 2 years of storage in artificial saliva at 37 °C. Nanoleakage evaluation and hybrid layer characterization were performed by SEM. Bond strength data was examined by three-way ANOVA followed by Tukey and Dunnett’s test (α = 0.05).

Results: Pretreatments significantly affected the ability of neat and solvated resins to bond to etched-dry dentin (p = 0.001). Ageing significantly lowered bond strengths depending on resin composition and DMSO-application times (p = 0.007). While hybridization of DMSO-treated dentin with the solvated resin produced no significant reductions in bond strengths after ageing (p < 0.05) improving hybrid layer integrity, direct bonding of the neat hydrophobic-rich resin matched the long-term bonding performance of the “gold standard” wet-bonding protocol (p > 0.05).

Significance: Lowering dentin’s hydration state via DMSO-dry bonding allows direct coupling of neat methacrylate-based resins, which may contribute to developing new strategies to ultimately extend the durability of resin-dentin interfaces.

Kokoelmat
  • Rinnakkaistallenteet [27094]

Turun yliopiston kirjasto | Turun yliopisto
julkaisut@utu.fi | Tietosuoja | Saavutettavuusseloste
 

 

Tämä kokoelma

JulkaisuajatTekijätNimekkeetAsiasanatTiedekuntaLaitosOppiaineYhteisöt ja kokoelmat

Omat tiedot

Kirjaudu sisäänRekisteröidy

Turun yliopiston kirjasto | Turun yliopisto
julkaisut@utu.fi | Tietosuoja | Saavutettavuusseloste