Evaluation of flexible three-dimensionally printed occlusal splint materials: An in vitro study

dc.contributor.authorPerea-Lowery Leila
dc.contributor.authorGibreel Mona
dc.contributor.authorGaroushi Sufyan
dc.contributor.authorVallittu Pekka
dc.contributor.authorLassila Lippo
dc.contributor.organizationfi=hammaslääketieteen laitos|en=Institute of Dentistry|
dc.contributor.organization-code1.2.246.10.2458963.20.64787032594
dc.converis.publication-id180707628
dc.converis.urlhttps://research.utu.fi/converis/portal/Publication/180707628
dc.date.accessioned2025-08-27T23:35:01Z
dc.date.available2025-08-27T23:35:01Z
dc.description.abstract<p><strong>Objective: </strong>To evaluate and compare the mechanical properties, water sorption, water solubility, and degree of double bond conversion of three different commercially available three-dimensional (3D) printing resins used for the fabrication of flexible occlusal splints.</p><p><strong>Methods: </strong>A digital printer was used to generate specimens from the evaluated splint materials (KeySplint Soft, IMPRIMO LC Splint flex, and V-Print splint comfort). The specimens were equally divided and tested either dry or after water storage at 37 °C for 30 days. A three-point bending test was used to assess flexural strength, elastic modulus, and fracture toughness. A two-body wear test was performed using a dual-axis chewing simulator. Water sorption and water solubility were measured after 30 days. The degree of double bond conversion was determined by FTIR-spectrometry. All data for the evaluated properties were collected and statistically analyzed.</p><p><strong>Results: </strong>Both material and storage conditions had a significant effect on the flexural strength (P < 0.001), elastic modulus (P < 0.001), fracture toughness (P < 0.001), and wear (P < 0.001). The highest water sorption was noticed with IMPRIMO LC Splint flex (1.9 ± 0.0 %), while V-Print splint comfort displayed the lowest water solubility (0.2 ± 0.0 %). For the degree of conversion, it was statistically non-significant among the different materials (P = 0.087).</p><p><strong>Significance: </strong>Different flexible 3D-printed splints available in the market displayed variations in the evaluated properties and clinicians should consider these differences when choosing occlusal device materials. Among the tested flexible splint materials, KeySplint Soft had the greatest flexural strength, elastic modulus, fracture toughness, wear resistance, and degree of conversion. It also showed the lowest water sorption.</p>
dc.identifier.jour-issn0109-5641
dc.identifier.olddbid204240
dc.identifier.oldhandle10024/187267
dc.identifier.urihttps://www.utupub.fi/handle/11111/52413
dc.identifier.urnURN:NBN:fi-fe2025082790369
dc.language.isoen
dc.okm.affiliatedauthorPerea, Leila
dc.okm.affiliatedauthorGibreel, Mona
dc.okm.affiliatedauthorGaroushi, Sufyan
dc.okm.affiliatedauthorVallittu, Pekka
dc.okm.affiliatedauthorLassila, Lippo
dc.okm.discipline313 Dentistryen_GB
dc.okm.discipline313 Hammaslääketieteetfi_FI
dc.okm.internationalcopublicationnot an international co-publication
dc.okm.internationalityInternational publication
dc.okm.typeA1 ScientificArticle
dc.publisher.countryUnited Statesen_GB
dc.publisher.countryYhdysvallat (USA)fi_FI
dc.publisher.country-codeUS
dc.relation.doi10.1016/j.dental.2023.08.178
dc.relation.ispartofjournalDental Materials
dc.source.identifierhttps://www.utupub.fi/handle/10024/187267
dc.titleEvaluation of flexible three-dimensionally printed occlusal splint materials: An in vitro study
dc.year.issued2023